← Back

Li5.7PS4.7Cl1.3
Good low-temperature performance, derived from optimized Li6PS5Cl composition.
Product Photo

XRD Pattern

Model Comparison
| D50 (μm) | Ionic Conductivity (S/cm) | Electronic Conductivity (S/cm) | Test Temperature(°C) | |
|---|---|---|---|---|
| Size A | 18.0±0.2 | 6.5±0.2 × 10⁻³ | 2.5±0.2 × 10⁻⁹ | 26 |
| Size B | 6.0±0.2 | 4.5±0.2 × 10⁻³ | 2.5±0.2 × 10⁻⁹ | 26 |
| Size C | 2.5±0.2 | 3.5±0.2 × 10⁻³ | 2.5±0.2 × 10⁻⁹ | 26 |
| Size D | 1.0±0.2 | 2.5±0.2 × 10⁻³ | 2.5±0.2 × 10⁻⁹ | 26 |
ICP Analysis(PPM)
| Na | Mg | K | Ca | Ti | Fe | Cu | Ni | |
|---|---|---|---|---|---|---|---|---|
| Li5.7PS4.7Cl1.3 | ≦200 | ≦50 | ≦150 | ≦10 | ≦100 | ≦10 | ≦50 | ≦10 |
Test data may vary slightly due to batch and testing condition differences. Please refer to the COA of the purchased batch for definitive specifications.